Characterisation of Liquation Products In A Nickel Base Superalloy
- Citation:
- K.M., O, Adeoye MO, Atanda PO, Olorunniwo OE, Aremo B.
2011. Characterisation of Liquation Products In A Nickel Base Superalloy. Ife Journal of Technology. 20:99–105., Number 2: IJT copy at www.tinyurl.com/y6ghbpl9